Wada et al., 2001 - Google Patents
Degradation of gas turbine blade materials in integrated coal-gasification combined cycle plantWada et al., 2001
- Document ID
- 8003291035407366520
- Author
- Wada K
- Yan L
- Takahashi M
- Takaishi K
- Furukawa T
- Publication year
- Publication venue
- Materials at High Temperatures
External Links
Snippet
Interest in the integrated coal-gasification combined cycle plant (IGCC) has increased because of its high efficiency. However, degradation of gas turbine component materials has not been studied so far. Therefore, the purpose of this study is to investigate the corrosion …
- 239000000463 material 0 title abstract description 31
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C28/00—Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- C23C28/30—Coatings combining at least one metallic layer and at least one inorganic non-metallic layer
- C23C28/32—Coatings combining at least one metallic layer and at least one inorganic non-metallic layer including at least one pure metallic layer
- C23C28/321—Coatings combining at least one metallic layer and at least one inorganic non-metallic layer including at least one pure metallic layer with at least one metal alloy layer
- C23C28/3215—Coatings combining at least one metallic layer and at least one inorganic non-metallic layer including at least one pure metallic layer with at least one metal alloy layer at least one MCrAlX layer
-
- F—MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING ENGINES OR PUMPS
- F01—MACHINES OR ENGINES IN GENERAL; ENGINE PLANTS IN GENERAL; STEAM ENGINES
- F01D—NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES
- F01D5/00—Blades; Blade-carrying members; Heating, heat-insulating, cooling or anti-vibration means on the blades or the members
- F01D5/12—Blades
- F01D5/28—Selecting particular materials; Particular measures relating thereto; Measures against erosion or corrosion
- F01D5/288—Protective coatings for blades
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C28/00—Coating for obtaining at least two superposed coatings either by methods not provided for in a single one of groups C23C2/00 - C23C26/00 or by combinations of methods provided for in subclasses C23C and C25C or C25D
- C23C28/30—Coatings combining at least one metallic layer and at least one inorganic non-metallic layer
- C23C28/34—Coatings combining at least one metallic layer and at least one inorganic non-metallic layer including at least one inorganic non-metallic material layer, e.g. metal carbide, nitride, boride, silicide layer and their mixtures, enamels, phosphates and sulphates
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02T—CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y02T50/00—Aeronautics or air transport
- Y02T50/60—Efficient propulsion technologies
- Y02T50/67—Relevant aircraft propulsion technologies
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C30/00—Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process
-
- F—MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING ENGINES OR PUMPS
- F01—MACHINES OR ENGINES IN GENERAL; ENGINE PLANTS IN GENERAL; STEAM ENGINES
- F01D—NON-POSITIVE DISPLACEMENT MACHINES OR ENGINES, e.g. STEAM TURBINES
- F01D25/00—Component parts, details, or accessories, not provided for in, or of interest apart from, other groups
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Hetmańczyk et al. | Advanced materials and protective coatings in aero-engines application | |
| JP2601964B2 (en) | Corrosion resistant magnesium titanate coating for gas turbine | |
| US20100237134A1 (en) | Repair process for coated articles | |
| EP1881154B1 (en) | Repair process for coated articles | |
| Stringer et al. | Current limitations of high-temperature alloys in practical applications | |
| US4374183A (en) | Silicon-slurry/aluminide coating | |
| Firouzi et al. | The structure and high temperature corrosion performance of medium-thickness aluminide coatings on nickel-based superalloy GTD-111 | |
| US20230340276A1 (en) | Chromate-Free Inorganic Coating Systems for Hot Corrosion Protection of Superalloy Substrate | |
| Natesan | Applications of coatings in coal-fired energy systems | |
| Toriz et al. | Thermal barrier coatings for jet engines | |
| Fu et al. | Microstructure and corrosion resistance of ERNiCrMo-13 and NiCrBSi coatings in simulated coal-fired boiler conditions: The effect of fly-ash composition | |
| Wada et al. | Degradation of gas turbine blade materials in integrated coal-gasification combined cycle plant | |
| US11535560B2 (en) | Chromate-free ceramic coating compositions for hot corrosion protection of superalloy substrates | |
| Simms et al. | Development of oxides at TBC–bond coat interfaces in burner rig exposures | |
| Wenglarz et al. | Chemical aspects of deposition/corrosion from coal-water fuels under gas turbine conditions | |
| Jinyang et al. | Corrosion Behavior of Austenitic stainless steels utilized for coal-fired boilers in simulated coal-ash/high sulfur environments | |
| GB2101910A (en) | Improvements in or relating to thermally protected alloys | |
| Bons et al. | High pressure turbine deposition in land based gas turbines from various synfuels | |
| McMinn et al. | Field evaluation of gas turbine protective coatings | |
| Peichl et al. | High‐temperature behavior of different coatings in high‐performance gas turbines and in laboratory tests | |
| Saricimen et al. | Hot corrosion behavior of plasma and HVOF sprayed Co-and Ni-based coatings at 900 C | |
| Nakamori et al. | Hot corrosion and its prevention in high temperature heavy oil firing gas turbines | |
| Whitlow et al. | Combustion turbine deposition observations from residual and simulated residual oil studies | |
| Le Zhou et al. | DEGRADATION OF (Ni, Pt) AI COATINGS BY MIXTURE OF SODIUM AND POTASSIUM SULFATE AT 950 C | |
| Malik et al. | The Corrosion Resistance of Protective Coatings |