JP2002070281A - Coating method for wall surface - Google Patents

Coating method for wall surface

Info

Publication number
JP2002070281A
JP2002070281A JP2000256878A JP2000256878A JP2002070281A JP 2002070281 A JP2002070281 A JP 2002070281A JP 2000256878 A JP2000256878 A JP 2000256878A JP 2000256878 A JP2000256878 A JP 2000256878A JP 2002070281 A JP2002070281 A JP 2002070281A
Authority
JP
Japan
Prior art keywords
wall surface
coating
temporary
filler
temporary hole
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2000256878A
Other languages
Japanese (ja)
Inventor
Toshiji Sako
利治 佐古
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Electric Works Co Ltd
Original Assignee
Matsushita Electric Works Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Matsushita Electric Works Ltd filed Critical Matsushita Electric Works Ltd
Priority to JP2000256878A priority Critical patent/JP2002070281A/en
Publication of JP2002070281A publication Critical patent/JP2002070281A/en
Pending legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To provide a coating method for a wall surface, capable of facilitating the repair of a temporary hole made in the wall surface and maintaining the durability of repaired sections on the wall surface by installing a temporary part in the wall surface and coating the wall surface with an antifouling coating material. SOLUTION: In the coating method for installing the temporary part in the wall surface 1 and coating the wall surface 1 with the antifouling coating material, a filler 3, wherein a coated film layer 6 composed of the antifouling coating material is formed on a surface side, is inserted for fixation into the temporary hole 2 made in the wall surface 1 for the purpose of fixing the temporary part when the temporary part is removed.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】本発明は、外壁等の壁面を現
場で塗装する塗装方法に関し、具体的には、壁面に仮設
部を固定しながら、この壁面に防汚性コーティング材料
を塗装し、その後この仮設部を撤去する際に、この壁面
に明けた仮設部を固定した仮設穴を補修する壁面への塗
装方法に関するものである。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a coating method for painting a wall surface such as an outer wall on site, and more specifically, applying an antifouling coating material to the wall surface while fixing a temporary portion to the wall surface. The present invention relates to a method of coating a wall surface for repairing a temporary hole for fixing a temporary portion drilled on the wall surface when removing the temporary portion.

【0002】[0002]

【従来の技術】外壁等の壁面を現場で塗装する際に、こ
の壁面に仮設部を設置して行うことが汎用されている。
この場合、仮設部を撤去する際に、この壁面に仮設部を
固定するために明けた仮設穴を補修する必要がある。こ
の補修作業は、安全等の観点から短時間で行うために、
充填材を埋め込み、その上から仕上げ塗料のみを塗装す
る方法が多用されている。
2. Description of the Related Art When a wall surface such as an outer wall is painted on site, it is widely used to install a temporary portion on the wall surface.
In this case, when removing the temporary part, it is necessary to repair a temporary hole that has been drilled to fix the temporary part to this wall surface. This repair work is performed in a short time from the viewpoint of safety, etc.
A method of embedding a filler and applying only a finish paint thereon is often used.

【0003】[0003]

【発明が解決しようとする課題】上記塗装方法では、仮
設穴を補修した壁面箇所の耐久性が、他の壁面に比較し
て低下している恐れがある。近年、外壁等の壁面に防汚
性を付与する塗料として、シリコーン樹脂等の無機塗料
に酸化チタン等の光触媒を含有した防汚性コーティング
材料が採用されている。上記光触媒を含有した塗料は、
塗装の際に、光触媒が外壁に悪影響をおよぼさないよう
下層にプライマー層を形成するなど、複数の層を形成し
ながら塗装する方法が採用されている。このような防汚
性コーティング材料にあっては、仮設穴を補修した箇所
の耐久性が劣ると、この箇所を基点として汚れが付着す
るため、壁面に塗装した塗膜全体の防汚性効果を低下さ
せてしまう恐れがある。
In the above coating method, there is a possibility that the durability of the wall portion where the temporary hole has been repaired is lower than that of other wall surfaces. 2. Description of the Related Art In recent years, an antifouling coating material containing a photocatalyst such as titanium oxide in an inorganic paint such as a silicone resin has been employed as a paint for imparting antifouling properties to a wall surface such as an outer wall. Paint containing the photocatalyst,
At the time of painting, a method of painting while forming a plurality of layers, such as forming a primer layer in a lower layer so that the photocatalyst does not adversely affect the outer wall, has been adopted. In such an antifouling coating material, if the durability of the portion where the temporary hole was repaired is poor, dirt will adhere from this portion as a starting point, and the antifouling effect of the entire coating applied to the wall surface will be reduced. There is a risk of lowering.

【0004】本発明は上記の事情に鑑みてなされたもの
で、その目的とするところは、壁面に仮設部を設置し、
この壁面に防汚性コーティング材料を塗装する塗装方法
にあって、壁面に明けた仮設穴の補修が容易にでき、補
修した壁面箇所の耐久性を保持することのできる壁面の
塗装方法を提供することにある。
The present invention has been made in view of the above circumstances, and a purpose thereof is to provide a temporary portion on a wall surface,
A coating method for coating an antifouling coating material on a wall surface, the method providing a coating method for a wall surface capable of easily repairing a temporary hole formed in the wall surface and maintaining durability of the repaired wall portion. It is in.

【0005】[0005]

【課題を解決するための手段】請求項1記載の壁面の塗
装方法は、壁面に仮設部を設置し、この壁面に防汚性コ
ーティング材料を塗装する塗装方法において、上記仮設
部を撤去する際に、この壁面に明けて仮設部を固定した
仮設穴に、上記防汚性コーティング材料からなる塗膜層
を表面側に形成した充填材を挿入して固着することを特
徴とする。上記によって、充填材を挿入することで作業
者が短時間で容易に補修をすることができるものであ
る。また、上記塗装方法は、上記充填材の表面側にあら
かじめ防汚性コーティング材料からなる塗膜層を形成し
ているので、仮設穴を塞ぎながら、この塞いだ壁面の箇
所に他と同様の防汚性を長期間保持することができるも
のである。
According to a first aspect of the present invention, there is provided a method for coating a wall, comprising the steps of: installing a temporary portion on the wall, and coating the wall with an antifouling coating material; Further, a filler having a coating layer made of the above antifouling coating material formed on the surface side is inserted and fixed in a temporary hole formed in the wall surface and fixing a temporary portion. As described above, the worker can easily perform repair in a short time by inserting the filler. In the above-mentioned coating method, since a coating layer made of an antifouling coating material is previously formed on the surface side of the above-mentioned filler, while blocking the temporary hole, a portion of the closed wall surface is protected similarly to the other. Stain can be maintained for a long time.

【0006】請求項2記載の壁面の塗装方法は、請求項
1記載の壁面の塗装方法において、上記塗膜層を形成し
た充填材の蓋部で、上記仮設穴の入口を覆うことを特徴
とする。上記によって、仮設穴の入口が破損していても
補修できるものである。また、上記塗装方法は、仮設穴
の内部に水等が浸入することを防止することができるも
のである。
According to a second aspect of the present invention, in the method for coating a wall according to the first aspect, the entrance of the temporary hole is covered with a lid of the filler on which the coating layer is formed. I do. As described above, even if the entrance of the temporary hole is damaged, it can be repaired. Further, the above-described coating method can prevent water or the like from entering the inside of the temporary hole.

【0007】請求項3記載の壁面の塗装方法は、請求項
1記載の壁面の塗装方法において、上記塗膜層を表面側
に形成した充填材が、この塗膜層を壁面と略平坦となる
ようにして上記仮設穴に嵌合することを特徴とする。上
記によって、充填材を挿入した壁面に凹凸がないため、
汚れが付着する基点が生じにくいものである。また、上
記塗装方法は、意匠性に優れた壁面に塗装することがで
きるものである。
According to a third aspect of the present invention, in the method for coating a wall according to the first aspect, the filler in which the coating layer is formed on the surface side makes the coating layer substantially flat with the wall. It is characterized in that it fits in the temporary hole in this way. By the above, because there is no unevenness on the wall surface where the filler is inserted,
A base point to which dirt adheres hardly occurs. In addition, the above-mentioned coating method can coat a wall surface having excellent design properties.

【0008】請求項4記載の壁面の塗装方法は、請求項
1乃至請求項3いずれか記載の壁面の塗装方法におい
て、上記充填材が、仮設穴にねじ止めされることを特徴
とする。上記によって、充填材が仮設穴に確実に固定さ
れ易くなると共に、短時間で仮設穴の補修をすることが
できるものである。
According to a fourth aspect of the present invention, in the method for coating a wall according to any one of the first to third aspects, the filler is screwed into the temporary hole. According to the above, the filler is easily fixed to the temporary hole reliably, and the temporary hole can be repaired in a short time.

【0009】請求項5記載の壁面の塗装方法は、請求項
1乃至請求項4いずれか記載の壁面の塗装方法におい
て、上記防汚性コーティング材料からなる塗膜層が、下
層にプライマー層を、上層に無機塗料に光触媒を含有し
た防汚層を形成したものであることを特徴とする。上記
によって、防汚性に優れる塗膜を壁面に形成することが
できるものである。
According to a fifth aspect of the present invention, in the method for coating a wall surface according to any one of the first to fourth aspects, the coating layer comprising the antifouling coating material comprises a primer layer as a lower layer, It is characterized in that an antifouling layer containing a photocatalyst in an inorganic paint is formed on the upper layer. According to the above, a coating film having excellent antifouling property can be formed on the wall surface.

【0010】[0010]

【発明の実施の形態】図1、2は、請求項1、2、5に
係る発明に対応する方法の実施の形態の一例を説明した
壁面の要部断面図、図2(a)は仮設部を設置した際の
壁面の要部断面図、図2(b)は仮設部を撤去した際の
壁面の要部断面図である。
1 and 2 are cross-sectional views of a main part of a wall for explaining an embodiment of a method according to the first, second and fifth aspects of the present invention, and FIG. FIG. 2B is a cross-sectional view of a main part of the wall surface when the temporary part is removed, and FIG.

【0011】外壁等の壁面1に現場で塗料を塗装する塗
装方法では、作業者が塗装作業を行うための足場12を
取付ける仮設部11を壁面に設置して作業を行う。その
ため、壁面1に仮設穴2をあけて、この仮設穴2に仮設
部11を固定する。本発明の塗装方法は、この仮設部1
1を撤去する際に、壁面1に明けて仮設部11を固定し
た仮設穴2を補修する方法である。
In a painting method for painting a paint on the wall surface 1 such as an outer wall, a worker installs a temporary portion 11 on which a scaffold 12 for performing painting work is installed on the wall surface. Therefore, a temporary hole 2 is formed in the wall surface 1 and the temporary portion 11 is fixed in the temporary hole 2. The coating method of the present invention uses the temporary part 1
This is a method of repairing a temporary hole 2 in which a temporary portion 11 is fixed by drilling in a wall surface 1 when removing 1.

【0012】上記塗装方法で使用する塗料は、防汚性コ
ーティング材料である。上記防汚性コーティング材料と
しては、例えば、シリコーン樹脂等の無機塗料に酸化チ
タン等の光触媒を含有したもの、塗料中にセラミック粒
子を分散させて水との接触角を小さくしたもの等が挙げ
られる。なかでも、光触媒を含有した防汚性コーティン
グ材料は、紫外線を照射すると光触媒の活性作用で汚れ
の成分である有機物を分解するので、太陽光が照射する
屋外で使用すると長期にわたって防汚性を保持する点で
優れるものである。上記防汚性コーティング材料は、塗
装を施す壁面1との密着性を良好にしたり、光触媒等が
壁面1に悪影響をおよぼさないように下層にプライマー
層18となる塗料を塗布して利用することが多い。な
お、図中の符号16は壁面に塗装した塗膜層、17は塗
膜層16の表面側に形成した防汚性コーティング材料か
らなる防汚層である。
The paint used in the above coating method is an antifouling coating material. Examples of the antifouling coating material include, for example, those containing a photocatalyst such as titanium oxide in an inorganic paint such as a silicone resin, and those in which ceramic particles are dispersed in the paint to reduce the contact angle with water. . Above all, antifouling coating materials containing photocatalysts degrade organic matter, which is a component of dirt, by the action of photocatalyst when irradiated with ultraviolet light. It is excellent in that it does. The antifouling coating material is used by applying a coating material to be a primer layer 18 on the lower layer so as to improve the adhesion to the wall surface 1 to be coated or to prevent a photocatalyst or the like from adversely affecting the wall surface 1. Often. In the drawing, reference numeral 16 denotes a coating layer applied to the wall surface, and 17 denotes an antifouling layer made of an antifouling coating material formed on the surface side of the coating layer 16.

【0013】本発明の塗装方法は、仮設部11を撤去す
る際に、壁面1に明けた仮設穴2に充填材3を挿入して
固着する。上記充填材3は、図1に示すように断面視で
略Tの字型をしたものであり、仮設穴2に挿入する脚部
4と、仮設穴2の入口を覆う蓋部5で形成されている。
上記脚部4は、仮設穴2の内径よりやや小さい外径を有
して、その形状が略円筒状の筒体である。上記蓋部5
は、仮設穴2の内径よりやや大きな外円周を有して、そ
の形状が略半円球状である。この蓋部5は、壁面1を塗
装したものと同様の防汚性コーティング材料からなる塗
膜層6が形成されている。この塗膜層6は、表面側とな
る上層に上記防汚性コーティング材料で形成した防汚層
7と、その下層にプライマー層8を有している。また、
上記充填材3の材料としては、耐久性を有するものであ
り、例えば、セメント系、セラミック系、ステンレス等
の金属系の材料が挙げられる。また蓋部5は、塗料との
密着性を高めるため、塗膜層6を形成する側に多少の凹
凸を有しているものが好ましい。
According to the coating method of the present invention, when removing the temporary portion 11, the filler 3 is inserted and fixed in the temporary hole 2 formed in the wall surface 1. The filler 3 has a substantially T-shape in cross section as shown in FIG. 1, and is formed by a leg 4 inserted into the temporary hole 2 and a lid 5 covering the entrance of the temporary hole 2. ing.
The leg 4 has an outer diameter slightly smaller than the inner diameter of the temporary hole 2 and is a substantially cylindrical tube. The lid 5
Has an outer circumference slightly larger than the inner diameter of the temporary hole 2, and has a substantially semi-spherical shape. The lid portion 5 has a coating layer 6 made of the same antifouling coating material as that obtained by coating the wall surface 1. The coating film layer 6 has an antifouling layer 7 formed of the above antifouling coating material on an upper layer on the surface side, and a primer layer 8 on a lower layer. Also,
The material of the filler 3 has durability, and examples thereof include metal materials such as cement, ceramic, and stainless steel. The lid 5 preferably has some irregularities on the side on which the coating layer 6 is formed in order to enhance the adhesion to the paint.

【0014】上記塗装方法は、仮設部11を撤去する際
に、仮設穴2に充填材3の脚部4を挿入し固着すると共
に、充填材3の蓋部5で仮設穴2の入口を覆う。上記充
填材3の固着は、仮設穴2及びその周囲にセメント、シ
−リング材、接着材等を挿入または塗布し、充填材3を
直ちに挿入することによってできるものである。上記塗
装方法は、蓋部5で仮設穴2の入口を覆うので、仮設穴
2の入口が破損していてもこれを補うことができ、ま
た、仮設穴2の内部に水等が浸入することを防止するこ
とができる。
According to the above-mentioned coating method, when removing the temporary portion 11, the leg portion 4 of the filler 3 is inserted and fixed in the temporary hole 2, and the lid 5 of the filler 3 covers the entrance of the temporary hole 2. . The filler 3 can be fixed by inserting or applying a cement, a sealing material, an adhesive or the like to the temporary hole 2 and its surroundings, and immediately inserting the filler 3. In the above-described coating method, since the entrance of the temporary hole 2 is covered with the lid portion 5, even if the entrance of the temporary hole 2 is damaged, it can be compensated for, and water or the like enters the inside of the temporary hole 2. Can be prevented.

【0015】なお、充填材3の蓋部5の形状は、上記略
半円球状以外でもよく、例えば、厚みの薄い円板状のも
のでもよい。
The shape of the lid 5 of the filler 3 may be other than the above-mentioned substantially semi-spherical shape. For example, it may be a thin disk.

【0016】図3は、請求項1、2、4、5に係る発明
に対応する方法の実施の形態の一例を説明した壁面の要
部断面図である。上記実施の形態と異なる点のみ説明す
る。
FIG. 3 is a sectional view of an essential part of a wall surface for explaining an example of an embodiment of a method according to the first, second, fourth and fifth aspects of the present invention. Only different points from the above embodiment will be described.

【0017】上記塗装方法に用いる充填材3は、その脚
部4にネジ9が形成されており、仮設穴2にねじ止めで
固着されるものである。この場合、上記仮設穴2は、仮
設部11をねじ止めで固定したものである。上記塗装方
法は、この仮設穴2に形成したネジ穴10に脚部4を差
し込み、ねじ止めで充填材3を固定する。上記塗装方法
は、充填材3が仮設穴2に確実に固定され易くなると共
に、短時間で仮設穴2の補修をすることができる。
The filler 3 used in the above coating method has a screw 9 formed in the leg 4 and is fixed to the temporary hole 2 by screwing. In this case, the temporary hole 2 is formed by fixing the temporary portion 11 with a screw. In the above-mentioned coating method, the leg 4 is inserted into the screw hole 10 formed in the temporary hole 2, and the filler 3 is fixed by screwing. According to the above-mentioned coating method, the filler 3 can be easily fixed to the temporary hole 2 reliably, and the temporary hole 2 can be repaired in a short time.

【0018】図4は、請求項1、3、5に係る発明に対
応する方法の実施の形態の一例を説明した壁面の要部断
面図である。上記実施の形態と異なる点のみ説明する。
FIG. 4 is a sectional view of an essential part of a wall surface for explaining an example of an embodiment of a method according to the first, third and fifth aspects of the present invention. Only different points from the above embodiment will be described.

【0019】上記塗装方法に用いる充填材3は、全体が
仮設穴2の内径よりやや小さい外径を有した略円筒状の
筒体14である。この筒体14は、固着した際の表面側
に、上述と同様に壁面1を塗装したものと同様の防汚性
コーティング材料からなる塗膜層6が形成されており、
また、上記筒体14は、仮設穴2に嵌合した際にこの塗
膜層6が壁面1と略平坦になるように長さを形成してい
る。上記塗装方法は、充填材3が、壁面1と略平坦にな
るように仮設穴2に嵌合されるので、充填材3を挿入し
た壁面1に凹凸ができないため、汚れが付着する基点が
生じ難く、また、意匠性に優れた塗装をすることができ
る。
The filler 3 used in the above coating method is a substantially cylindrical tubular body 14 having an outer diameter slightly smaller than the inner diameter of the temporary hole 2. This cylindrical body 14 has a coating layer 6 made of the same antifouling coating material as that obtained by painting the wall surface 1 in the same manner as described above, on the surface side when it is fixed,
The tubular body 14 has a length such that the coating layer 6 is substantially flat with the wall surface 1 when fitted into the temporary hole 2. In the above-mentioned coating method, the filling material 3 is fitted into the temporary hole 2 so as to be substantially flat with the wall surface 1, so that the wall surface 1 into which the filling material 3 is inserted cannot be uneven, so that a base point to which dirt adheres is generated. It is difficult to apply, and it is possible to paint with excellent design.

【0020】本発明の塗装方法は、充填材3を仮設穴2
に挿入することで、短時間で容易に補修をすることがで
きる。また、上記塗装方法は、上記充填材3の表面側に
あらかじめ防汚性コーティング材料からなる塗膜層6を
形成しているので、仮設穴2を塞ぎながら、この塞いだ
壁面1の箇所に他と同様の防汚性を長期間保持すること
ができる。
In the coating method of the present invention, the filler 3 is
Can be easily repaired in a short time. Further, in the coating method, since the coating layer 6 made of the antifouling coating material is formed in advance on the surface side of the filler 3, the temporary hole 2 is closed, The same antifouling property can be maintained for a long time.

【0021】[0021]

【発明の効果】請求項1〜5記載の壁面の塗装方法は、
防汚性コーティング材料からなる塗膜層を表面側に形成
した充填材を仮設穴に挿入して固着するので、壁面に明
けた仮設穴の補修が容易にでき、また、補修した箇所の
防汚性を長期間保持することができる。
The method for coating a wall according to claims 1 to 5,
Since the filler formed on the surface side with the coating layer made of the antifouling coating material is inserted and fixed in the temporary hole, the temporary hole drilled in the wall surface can be easily repaired, Property can be maintained for a long time.

【0022】さらに、請求項2記載の壁面の塗装方法
は、特に、蓋部で仮設穴の入口を覆うので、仮設穴の入
口が破損していてもこれを補うことができ、また、仮設
穴の内部に水等が浸入することを防止することができ
る。
Furthermore, in the method for coating a wall surface according to the second aspect, since the entrance of the temporary hole is particularly covered with the lid, even if the entrance of the temporary hole is damaged, it can be compensated. It is possible to prevent water or the like from entering the inside of the device.

【0023】さらに、請求項3記載の壁面の塗装方法
は、特に、充填材が、壁面と略平坦になるように仮設穴
に嵌合されるので、充填材を挿入した壁面に凹凸ができ
ないため、汚れが付着する基点が生じ難く、また、意匠
性に優れた塗装をすることができる。
Furthermore, in the method for coating a wall surface according to the third aspect, since the filler is fitted into the temporary hole so as to be substantially flat with the wall surface, the wall surface into which the filler is inserted cannot be uneven. In addition, a base point to which dirt adheres hardly occurs, and coating with excellent design can be performed.

【0024】さらに、請求項4記載の壁面の塗装方法
は、特に、充填材が仮設穴に固定され易くなると共に、
短時間で仮設穴の補修をすることができる。
Furthermore, the method for coating a wall according to the fourth aspect is particularly advantageous in that the filler is easily fixed to the temporary holes.
The temporary hole can be repaired in a short time.

【0025】さらに、請求項4記載の壁面の塗装方法
は、特に、防汚性に優れる塗膜を壁面に形成することが
できる。
Furthermore, the method for coating a wall according to claim 4 can form a coating film having excellent antifouling property on the wall.

【図面の簡単な説明】[Brief description of the drawings]

【図1】本発明を用いた実施の形態の一例を説明した壁
面の要部断面図である。
FIG. 1 is a sectional view of a main part of a wall surface for explaining an example of an embodiment using the present invention.

【図2】(a)は仮設部を設置した際の壁面の要部断面
図であり、(b)は仮設部を撤去した際の壁面の要部断
面図である。
FIG. 2A is a sectional view of a main part of a wall surface when a temporary part is installed, and FIG. 2B is a sectional view of a main part of a wall surface when the temporary part is removed.

【図3】本発明を用いた他の実施の形態の一例を説明し
た壁面の要部断面図である。
FIG. 3 is a cross-sectional view of a main part of a wall surface illustrating an example of another embodiment using the present invention.

【図4】本発明を用いた他の実施の形態の一例を説明し
た壁面の要部断面図である。
FIG. 4 is a cross-sectional view of a main part of a wall surface illustrating an example of another embodiment using the present invention.

【符号の説明】[Explanation of symbols]

1 壁面 2 仮設穴 3 充填材 6 塗膜層 11 仮設部 DESCRIPTION OF SYMBOLS 1 Wall surface 2 Temporary hole 3 Filler 6 Coating layer 11 Temporary part

Claims (5)

【特許請求の範囲】[Claims] 【請求項1】 壁面に仮設部を設置し、この壁面に防汚
性コーティング材料を塗装する塗装方法において、上記
仮設部を撤去する際に、この壁面に明けて仮設部を固定
した仮設穴に、上記防汚性コーティング材料からなる塗
膜層を表面側に形成した充填材を挿入して固着すること
を特徴とする壁面への塗装方法。
In a coating method in which a temporary portion is provided on a wall surface and an antifouling coating material is applied to the wall surface, when the temporary portion is removed, a temporary hole is formed in the wall surface and the temporary portion is fixed. A method of coating a wall surface, comprising inserting and fixing a filler having a coating layer formed of the above-mentioned antifouling coating material on the surface side.
【請求項2】 上記塗膜層を形成した充填材の蓋部で、
上記仮設穴の入口を覆うことを特徴とする請求項1記載
の壁面への塗装方法。
2. The lid of the filler on which the coating layer is formed,
2. The method for coating a wall surface according to claim 1, wherein an entrance of the temporary hole is covered.
【請求項3】 上記塗膜層を表面側に形成した充填材
が、この塗膜層を壁面と略平坦となるようにして上記仮
設穴に嵌合することを特徴とする請求項1記載の壁面へ
の塗装方法。
3. The temporary hole according to claim 1, wherein the filler having the coating layer formed on the surface side is fitted into the temporary hole such that the coating layer becomes substantially flat with the wall surface. How to paint on the wall.
【請求項4】 上記充填材が、仮設穴にねじ止めされる
ことを特徴とする請求項1乃至請求項3いずれか記載の
壁面への塗装方法。
4. The method according to claim 1, wherein the filler is screwed into the temporary hole.
【請求項5】 上記防汚性コーティング材料からなる塗
膜層が、下層にプライマー層を、上層に無機塗料に光触
媒を含有した防汚層を形成したものであることを特徴と
する請求項1乃至請求項4いずれか記載の壁面への塗装
方法。
5. A coating layer comprising the antifouling coating material, wherein a primer layer is formed as a lower layer, and an antifouling layer containing a photocatalyst in an inorganic coating is formed as an upper layer. A method for coating a wall surface according to any one of claims 1 to 4.
JP2000256878A 2000-08-28 2000-08-28 Coating method for wall surface Pending JP2002070281A (en)